EFFECT OF POST HEAT TEMPERATURE TO HARDNESS AND MACROSTRUCTURE IN WELDED STELL ST 37

Abstract: The present study aims to investigate the effect of post heat temperature of hardness and macrostructure on the result steel welded St 37. Welded process with SMAW (Shelded Metal Arc Welding) and AC-DC current. Plate steel ST 37 welded of longitudinal, than heat treatment with temperature various:300°C, 400°C dan 500°C. Highest rate hardness 157,83 kg/mm2 on temperature treatment spesiment 500ocause have ferit grain boundary structure more and homogen so properties more hardness. The lows bending strength 43,51 kg/mm2on raw material, cause have ferit structure and perlit so more soft properties.The micostuctrure welded area arround; ferit graind boundary, ferit widmans tatten, ferit acicular and perlit.
Key Word: SteelSt 37, SMAW, post heat, and hardness
Penulis: Subardi, Djoko Suprijanto, Roza Lyndu R. Mahendra