Abstract: A method developed
to predict the failure that occurs at gas transmission pipe caused by loading
with peak angle crack opening is described in this paper. There are two aspects
become the main consideration; the maximum crack peak angle opening for the
given load and space, and the determination of the critical stress intensity
factor to search at what degree of loading the crack on the gas transmission
pipe experiencing creep or failure. This research uses arc-shaped tension
specimen and the analysis is carried out by finite element method using ansys ™
rel 5.4. In order to get the stress intensity factor, the loading is varied
from 1 KN to 160 KN. Based on finite element method, the maximum stress
intensity factor occurs at the range of loading of 16-160 KN, which is 5.67 x
1016 MPa.m1/2, and the minimum factor occurs at the range of loading of 0.5-1
KN, which is 3.76 MPa.m1/2. The stress intensity factor result is also
validated with the analytical result. The maximum crack peak angle opening
occurs at the range of loading of 16-160 KN which is 250, the stage that is
able to cause pipe failure.
Keywords: Stress Intensity
Factor;Maximum Crack Peak Angle Opening;Finite Element Method;Arc-shaped
Tension
Penulis: Asbar R